NBN EN 12502-3:2005

Protection of metallic materials against corrosion - Guidance on the assessment of corrosion likelihood in water distribution and storage systems - Part 3: Influencing factors for hot dip galvanised ferrous materials

ACTIVE

About this standard

Languages
German, English and French
Type
NBN
Status
ACTIVE
Publication date
26 January 2005
ICS Code
23.040.99 (Other pipeline components)
77.060 (Corrosion of metals)
91.140.60 (Water supply systems)
Withdrawn Date
Price
€ 89,00

About this training

Summary

This document gives a review of influencing factors of the corrosion likelihood of hot dip galvanized steel and cast iron, used as tubes, tanks and equipment, unalloyed and low alloy ferrous materials in water distribution and storage systems as defined in EN 12502-1.