NBN EN 13674-1:2011

Railway applications - Track - Rail - Part 1: Vignole railway rails 46 kg/m and above

WITHDRAWN

About this standard

Languages
English and French
Type
NBN
Standards committee
CEN/TC 256
Status
WITHDRAWN
Publication date
23 March 2011
Amended By
EN 13674-1:2011/FprA1
ICS Code
93.100 (Construction of railways)
Withdrawn Date
07 March 2023
Price
€ 50,00

About this training

Summary

This European Standard specifies Vignole railway rails of 46 kg/ m and greater linear mass, for conventional and high speed railway track usage.
Nine pearlitic steel grades are specified covering a hardness range of 200 HBW to 440 HBW and include non heat treated non alloy steels, non heat treated alloy steels, and heat treated non alloy steels and heat treated alloy steels .
There are 23 rail profiles specified in this standard.
Two classes of rail straightness are specified, differing in requirements for straightness, surface flatness and crown profile. Two classes of profile tolerances are specified.