NBN EN 12513:2011

Founding - Abrasion resistant cast irons

ACTIVE

About this standard

Languages
German, English and French
Type
NBN
Standards committee
CEN/TC 190 (Foundry technology)
Status
ACTIVE
Publication date
23 March 2011
ICS Code
77.080.10 (Irons)
Withdrawn Date
Price
€ 121,00

About this training

Summary

This European Standard defines the grades of abrasion resistant white cast irons. It specifies the grades in terms of:
- chemical composition
- hardness.
The types of abrasion resistant white cast irons covered by this standard are:
a) unalloyed or low alloy cast irons
b) nickel-chromium cast irons covering two general types:
- 4 % Ni 2 % Cr cast irons
- 9 % Cr 5 % Ni cast irons
c) high chromium cast irons covering four ranges of chromium content:
- 11 % < Cr < / = 14 %
- 14 % < Cr < / = 18 %
- 18 % < Cr < / = 23 %
- 23 % < Cr < / = 30 %.
This European Standard does not define the abrasion resistant grades of ausferritic spheroidal graphite cast irons which are subject of EN 1564.