NBN EN 1366-6:2005

Fire resistance tests for service installations - Part 6: Raised access and hollow core floors

ACTIVE

About this standard

Languages
German, English and French
Type
NBN
Status
ACTIVE
Publication date
15 December 2004
ICS Code
13.220.50 (Fire-resistance of building materials and elements)
Withdrawn Date
Price
€ 89,00

About this training

Summary

This Part of EN 1366 specifies a method for determining the fire resistance of raised access floors and hollow floors when subjected to a fire from within the plenum beneath the floor. The fire exposure applied to the test specimen may be either:
a) standard time temperature curve
b) ' reduced' time temperature curve which follows the standard time/ temperature curve only up to 500 °C. After this temperature has been reached the temperature within the furnace is maintained at 500 °C.
This document does not determine the fire resistance of the sub-floor on which the raised or hollow floor is constructed this is given in EN 1365-2.